Nanoindentation simulations for copper and tungsten with adaptive-precision potentials
David Immel, Matous Mrovec, Ralf Drautz, Godehard Sutmann
The archive published only this paper's code-link row. Authors, date and abstract are from arXiv's metadata (CC0), read from the Kaggle arXiv metadata snapshot of 2026-09-12 where its title matched the archive's; the title is the archive's.
We perform nanoindentation simulations for both the prototypical face-centered cubic metal copper and the body-centered cubic metal tungsten with a new adaptive-precision description of interaction potentials including different accuracy and computational costs: We combine both a computationally efficient embedded atom method (EAM) potential and a precise but computationally less efficient machine learning potential based on the atomic cluster expansion (ACE) into an adaptive-precision (AP) potential tailored for the nanoindentation. The numerically expensive ACE potential is employed selectively only in regions of the computational cell where large accuracy is required. The comparison with pure EAM and pure ACE simulations shows that for Cu, all potentials yield similar dislocation morphologies under the indenter with only small quantitative differences. In contrast, markedly different plasticity mechanisms are observed for W in simulations performed with the central-force EAM potential compared to results obtained using the ACE potential which is able to describe accurately the angular character of bonding in W due to its half-filled d-band. All ACE-specific mechanisms are reproduced in the AP nanoindentation simulations, however, with a significant speedup of 20-30 times compared to the pure ACE simulations. Hence, the AP potential overcomes the performance gap between the precise ACE and the fast EAM potential by combining the advantages of both potentials.
Code
Repository list and official/mentioned flags are the archive's, frozen 2025-07-28. Reachability, where shown, is from one Syntology probe window (2026-09-16 to 2026-09-18); repositories not probed show nothing. GitHub stars are not tracked.
Code Syntology ran Syntology
Not run by Syntology. Nothing on this page verifies that the listed code works.
Results from the paper archive 2025-07-28
No leaderboard rows for this paper in the archive.
Report a problem or propose a change · a person checks every report against the paper or source before anything changes; decisions are listed on /corrections