{"about":{"site":"https://codewithpapers.app","non_affiliation":"Code with Papers and Syntology are not affiliated with, endorsed by, or sponsored by Papers with Code, Meta, or the pwc-archive mirror.","licence":"CC BY-SA 4.0","licence_url":"https://creativecommons.org/licenses/by-sa/4.0/legalcode","attribution":"https://codewithpapers.app/attribution","modified":"archive material modified by Syntology; see the attribution page"},"url":"/paper/nanoindentation-in-multi-modal-map","title":"Nanoindentation in multi-modal map combinations: A Correlative Approach to Local Mechanical Property Assessment","arxiv_id":"2008.12267","date":"2020-08-27","proceeding":null,"authors":["C. M. Magazzeni","H. M. Gardner","I. Howe","P. Gopon","J. C. Waite","D. Rugg","D. E. J. Armstrong","A. J. Wilkinson"],"abstract":"A method is presented for the registration and correlation of intrinsic property maps of materials, including data from nanoindentation hardness, Electron Back-Scattered Diffraction (EBSD), Electron Micro-Probe Analysis (EPMA). This highly spatially resolved method allows for the study of micron-scale microstructural features, and has the capability to rapidly extract correlations between multiple features of interest from datasets containing thousands of datapoints. Two case studies are presented in commercially pure (CP) titanium: in the first instance, the effect of crystal anisotropy on measured hardness and, in the second instance, the effect of an oxygen diffusion layer on hardness. The independently collected property maps are registered us-ing affine geometric transformations and are interpolated to allow for direct correlation. The results show strong agreement with trends observed in the literature, as well as providing a large dataset to facilitate future statistical analysis of microstructure-dependent mechanisms.","url_abs":"https://arxiv.org/abs/2008.12267v2","url_pdf":"https://arxiv.org/pdf/2008.12267v2.pdf","source":{"archive":"pwc-archive (Hugging Face), CC BY-SA 4.0","snapshot":"2025-07-28","licence_url":"https://creativecommons.org/licenses/by-sa/4.0/legalcode","row_kind":"links_only","authors_date_abstract":"arXiv metadata, CC0 1.0 (https://info.arxiv.org/help/license), from the Kaggle arXiv metadata snapshot of 2026-09-12"},"code_links":[{"paper_slug":"nanoindentation-in-multi-modal-map","repo_url":"https://github.com/cmmagazz/XPCorrelate","is_official":1,"mentioned_in_paper":1,"mentioned_in_github":0,"framework":"none","reach":null}],"tasks":[],"methods":[],"datasets_introduced":[],"methods_introduced":[],"results":[],"syntology":{"atlas_url":null,"mcp":null,"developers":"https://syntology.ai/developers"},"arxiv_metadata":null,"syntology_extracted_results":null}